What is the technique for daubing the 100P?

When recoating, repeatedly daub with each coat's thickness kept to about 5 mm.
Daub it so that the thickness of a single layer is 30 mm or less. Once it is significantly daubed, the pallet pressure becomes lower, causing curtaining.